A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Electroless Cu plating
Electroless Cu plating
2008-06-27
Cassie Iany
2008-06-27
shay kaplan
2008-06-27
Gord Wang
Electroless Cu plating
Cassie Iany
2008-06-27
Hello,

I am doing Electroless Cu plating on SiO2 substrate. I found the solution can
deposit Cu film on Si but not SiO2. I tried to use different self-assembly
monolayer to modify the surface, but still not succeed. One thing I am concerned
about the SiO2 substrate cleaned with Pirana solution has contact angle of 45
degree which is different from other reported contact angle (nearly Zero
degree). I don't know how the difference comes.

Appreciate if you share your experience and suggestion.

Regards

Cassie
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
The Branford Group
University Wafer