Artola, Juan Mari
piezorresistance stability
Artola, Juan Mari
1998-09-14
Hello everybody,

I am working in a project in which I am integrating some piezorresistances
of P-type on N-type substrates. The dopant I am using is a Filmtronics
spin-on dopant, called B-20. I use 1um thermal silicon dioxide as a
difussion mask and  the difussion process consists in a deposition phase of
1 hour at 850ºC and a distribution phase of 1 hour at 950ºC. I use 1um
aluminium layer as metalization and an annealing of 1hour at 450ºC.
After all this process I am having some stability problems. The value of the
integrated resistances vary on time.

Does anybody know which could be the problem? Could anybody help me somehow?

Thank you very much in advance.

Juan-Mari Artola
Microelectronics department
CEIT


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMStaff Inc.
Tanner EDA by Mentor Graphics