MEMSnet Home: MEMS-Talk: pdms removal
pdms removal
2008-06-28
Jose Guevarra
2008-06-28
Mohd.Yusuf
pdms removal
Jose Guevarra
2008-06-28
Hi,

  I use a silicon wafer with su-8 as a mold in a petri dishfor PDMS.
After the PDMS is solidified I remove it by peeling it off.

How do I thoroughly clean off the solidified PDMS from the wafer and
petri dish?

Thanks.
reply