Dave
2008-07-16
Hello,

I am looking to deposit an insulating, optically clear, layer for some
circuitry, and was wondering if I could Ebeam evaporate Silicon nitride?
Also, if I can, I saw something about alpha and beta forms, is there any
substantial difference when dealing with the insulating properties?

Thanks,
David Casale
Drexel University
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing