what is the problem with our STS ICP?
2008-09-19
[email protected]
2008-09-19
Andreas Fischer
2008-09-19
乔大勇
2008-09-19
[email protected]
what is the problem with our STS ICP?
[email protected]
2008-09-19
Hi, We have a STS ICP, working fine until recently.

Problem is when using pure gas, such as O2 or CF4 alone, then plasma is
stable. However if using mixed gas, O2+CF4, then plasma unstable. Lower
top coil power helps but etch rate would be much slower compare to before.

Can someone give a suggestion? Thanks.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
Process Variations in Microsystems Manufacturing
MEMS Technology Review