A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Filling deep vias with resist
Filling deep vias with resist
2008-10-27
Black, Robert
2008-10-28
Suzanne Scullen Ericson
2008-10-28
Jan Newman
2008-10-28
Robert Black
2008-10-28
Kevin Paul Nichols
2008-10-29
Michael D Martin
2008-10-29
汪飞
2008-10-27
[email protected]
Filling deep vias with resist
Robert Black
2008-10-28
Thanks for the replies.

I am definitely trapping air in the vias. I have
tried doing a PGMA puddle (resist solvent) to let it fill the via, and
follow with resist and have it wick down the via. X-sections appear to show
that the PGMA didn't reach the bottom of the via. I assume some sort of
de-wetting. I'd love to try spray, but capital expenditures are frozen.

I'm trying to fill and planerize the top side before backside pattern.

Robert

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Jan Newman
Sent: Tuesday, October 28, 2008 5:58 AM
To: 'General MEMS discussion'
Subject: Re: [mems-talk] Filling deep vias with resist

Hi Robert,

         Do you need to fill them or merely protect the internal surfaces?
If only protection required the EVG Nanospray will do the job.
If you need to fill them then the spray can act to initially wet the
internal surfaces and help fill during coating.

Jan
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
The Branford Group
Tanner EDA by Mentor Graphics