MEMSnet Home: MEMS-Talk: SiO2 deposition
SiO2 deposition
2008-11-21
[email protected]
2008-11-21
SEBESTA Edward
2008-11-21
John Hilton
2008-11-21
SEBESTA Edward
2008-11-23
Konstantin Glukh
2008-11-23
Tom Rust
2008-11-24
Juergen Leib - GMX
SiO2 deposition
Juergen Leib - GMX
2008-11-24
We did a project with them applying 100um (!) thick oxide layer on top of
Silicon Carbide.

As a standard process we do up 10 - 30µm and – actually the most important
thing - can control the stresses of the deposited  layer. The process is an
modified e-beam deposition (as suggested by John) and it is reasonable fast.

It also would be possible to structure the layer as well (contact opening
etc.) – is this an requirement for you?

Dr. Juergen Leib
MSG Lithoglas AG
Gustav-Meyer-Allee 25
D13355  Berlin (Germany)
Main:     +49 30 46403-618
eMail:   [email protected]
  www.lithoglas.de
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
MEMStaff Inc.