AZ 9260
2008-12-02
Hyun C Jung
2008-12-03
Oakes Garrett
2008-12-02
Hyun C Jung
2008-12-02
DaddiO
2008-12-03
Hennemeyer, Marc
AZ 9260
Hyun C Jung
2008-12-02
This is my parameters for AZ 9260.

1. Spin coat AZ 9260 at 3000 rpm for 1 min.
2. Soft bake for 90s
3. Expose 15s i-line4
4. Develop 3 min in AZ 400k 1:4