Au electroplating on Al substrate
2009-01-07
Denis Petrov
2009-01-07
Alexandre BOE
2009-01-07
Oakes Garrett
2009-01-08
Ravi Shankar
2009-01-08
IGOR KADIJA
2009-01-08
Heather Broadbent
2009-01-08
Edward Sebesta
2009-01-08
Wilson, Thomas
2009-01-08
Brad Cantos
2009-01-08
Huihang Dong
Au electroplating on Al substrate
Ravi Shankar
2009-01-08
Hi Denis Petrov,

               I came across a similar situtation before and yes, Au
was not electroplated on to the Aluminum substrate... in my
experiment, a sulfite based Au plating solution was used, and even
after 1 hour,   au was not plated on al substrate... i guess it may be
becos of adhesion related issues, since Au was getting plated on Cr
substrate (however, surafce quality of plated gold on Cr substrate was
poor).... interested to know the exact reason, if anyone can explain..

Regards,
A. Ravi Shankar,
Senior Research Scholar,
Microelectronics and MEMS Lab,
Electronics & ECE Department,
IIT Kharagpur.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer