Adhesion on Alumina
Gary Hillman
2009-01-16
Evelyn, it would seem to me that the Ti seed layer might be oxidized and
therefore the upper metal layers aren't sticking.  Is the surface discolored
by Ti and the metal above lifting off.  Gary

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of shay kaplan
Sent: Friday, January 16, 2009 8:39 AM
To: [email protected]; 'General MEMS discussion'
Subject: Re: [mems-talk] Adhesion on Alumina


Evelyn
How are you preparing the substrate surface before evap?
Shay

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics