MEMSnet Home: MEMS-Talk: front back photolitography
front back photolitography
2009-01-18
Andrea Mazzolari
2009-01-18
Bill Moffat
2009-02-04
DaddiO
2009-01-19
Reza Rashidi
front back photolitography
Bill Moffat
2009-01-18
There are a number of commercial aligners that can align front and back
to within submicron accuracy.  All you need to do is to locate a company
that has one.  Most of the aligners I know off that can do this are
contact aligners, if contact alignment is acceptable you should have no
problems.  If you have any problems contact me I know most of the
companies that manufacture these aligners.

Bill Moffat

________________________________

From: [email protected] on behalf of Andrea Mazzolari
Sent: Sun 1/18/2009 2:37 AM
To: General MEMS discussion
Subject: [mems-talk] front back photolitography


Hello all,
i need to perform front and back photolitography.

On each side of a 4'' silicon wafer i need to realize geometries of size
10um. Geometries on the opposite wafer faces must be aligned with the =
best
possible accuracy.
Here we don't have the possibility to realize front-back photolitography
and so i plan to ask to some company to do the job for me.

Which is the best precision accuracy which can be obtained on the market

Best regards,
Andrea

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
MEMS Technology Review
Harrick Plasma, Inc.