MEMSnet Home: MEMS-Talk: glass cracking during anodic bonding
glass cracking during anodic bonding
2009-02-26
jingru zhang
2009-02-26
Mehmet Aykol
2009-02-26
jingru zhang
2009-02-27
shay kaplan
2009-02-27
jingru zhang
2009-02-28
shay kaplan
2009-02-27
Staller, Steven E
2009-02-27
jingru zhang
2009-02-27
Brad Johnson
2009-02-27
jingru zhang
2009-03-02
Brad Johnson
2009-03-03
jingru zhang
2009-03-04
Brad Johnson
glass cracking during anodic bonding
jingru zhang
2009-02-27
I have different dimensions. For example, the width of the channel is 200
microns, and the depth is 100 microns.

On Fri, Feb 27, 2009 at 12:20 AM, shay kaplan  wrote:

> How wide and deep are your channels?

--
Jingru
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
University Wafer
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing