Dear all,

We are trying to spincoat Nusil CF19-2186 elastomer. We are facing problems
because the liquid is highly viscous and I think it starts to cure while we
are trying to degass it. The mixing of the base and the curing agent also
causes a lot of bubbles, so we think it is essential that we degass it
before spincoating. We are also trying to coat without degassing with mixed
results.

Any suggestions?.

thank you for the response
Allwyn.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Mentor Graphics Corporation
University Wafer