Hi,

Best way to solve these problem is to use a caustic etchant. An
excellent one is to use CuSO4 mixed with Ammonia. It will build a
tetra-ammin complex Cu(NH3)4++ which is the active etchant of the
Copper. It will never attac Nickel.

Best regards

Armin

______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
The Branford Group