MEMSnet Home: MEMS-Talk: Bearing holes in pyrex/glass wafers
Bearing holes in pyrex/glass wafers
2009-05-01
김태진
2009-05-01
Mehmet Aykol
2009-05-01
Kirt Williams
2009-05-02
Brian Stahl
2009-05-02
[email protected]
2009-05-02
Xiaoguang Liu
2009-05-02
Jackgong Hotmail
2009-05-02
HENRI FLECHNER
2009-05-03
Jackgong Hotmail
2009-05-04
Fei Wang
2009-05-04
Robert MacDonald
2009-05-06
김태진
2009-05-04
%Mihaela Carp
2009-05-02
HENRI FLECHNER
2009-05-03
tarun mudgal
2009-05-05
Jackgong Hotmail
2009-05-04
Tomblin, Graham
Bearing holes in pyrex/glass wafers
[email protected]
2009-05-02
TJ,

I always liked micro abrasive powder blasting for quick turn prototype work.

Jim


-----Original Message-----
From: 김태진 
To: [email protected]
Sent: Fri, 1 May 2009 3:31 pm
Subject: [mems-talk] Bearing holes in pyrex/glass wafers


Hi all!
I'm trying to think of a way to make a 2mm diameter through hole in a pyrex
afer.
I thought of etching the hole with DRIE, but thought it was inefficient and time
onsuming.
It also seems that I can't use conventional drilling machines to bear holes in
he pyrex as the substrate is to brittle.
Does anyone know how to drill holes in pyrex/glass wafers?
The features don't have to be too accurate..
Thanks!
TJ
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing