MEMSnet Home: MEMS-Talk: COC bonding
COC bonding
2009-05-20
Gareth Jenkins
COC bonding
Gareth Jenkins
2009-05-20
Hi

Does anyone have any experience of bonding Topas COC (8007x10)?
I haven't had any luck with pure thermal bonding in a heated press and
oxygen plasma treatment didn't help either. I also tried a solvent assisted
method (hexadecane + IPA) which stuck a little bit but not much.
N.B. I have to use 8007 so I can't use a lower Tg grade as an intermediate
layer and I have some quite shallow channels in my structure which makes it
harder.

If anyone has any good recipes, process tips or references that would be
great.

Gareth
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMS Technology Review
University Wafer