A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Hydrophobic recovery of PDMS
Hydrophobic recovery of PDMS
2009-05-30
DEBASHIS MAJI
2009-06-01
Bill Moffat
Hydrophobic recovery of PDMS
DEBASHIS MAJI
2009-05-30
Hi All,

I have a doubt regarding the hydrophobic recovery of PDMS. It is explained
that the hydrophobic recovery is due to the slow diffusion of the Lower
molecular weight PDMS components to the top surface thus rendering the
surface hydrophobic again. Here I have a doubt regarding, which lower
molecular weight ( compared to which heavier MW ) gets diffused in? Is it
the -CH3 ( MW-15) polymeric chain that slowly diffuses in to replace the
hydrophilic -OH group ( MW-17)?  Any sort of help shall be highly
appreciated.

Thanking you,

Debashis Maji, JRF,
School of Medical Science & Technology,
IIT Khargpur, India - 721302
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Mentor Graphics Corporation
The Branford Group