MEMSnet Home: MEMS-Talk: Dry etch of Gadolinium Gallium Garnet substrate
Dry etch of Gadolinium Gallium Garnet substrate
2009-06-04
Andrea Lucibello
Dry etch of Gadolinium Gallium Garnet substrate
Andrea Lucibello
2009-06-04
Hi all,

Can someone suggest a method to etch a GGG substrate (Gadolinium Gallium Garnet)
with RIE?What kind of gas is necessary?

Thanks in advance.
Regards

Dr. Andrea Lucibello
Junior Researcher
CNR - Istituto per la Microelettronica e Microsistemi
Area della Ricerca di Roma 2 - Tor Vergata
Via del Fosso del Cavaliere, 100 - 00133 Roma
Tel +39 0649934577 (Office)
Tel +39 0649934496   (Laboratory)
Mobile +39 3348314970
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Mentor Graphics Corporation
Nano-Master, Inc.