MEMSnet Home: MEMS-Talk: metallization on PDMS
metallization on PDMS
2009-06-01
nidhi maheshwari
2009-06-01
Pavan Samudrala
2009-06-01
Barbara Cortese
2009-06-03
nidhi maheshwari
2009-06-03
Joshua Tice
2009-06-03
Ruiz, Marcos Daniel (SENCOE)
2009-06-03
Barbara Cortese
2009-06-04
nidhi maheshwari
2009-06-04
Barbara Cortese
2009-06-04
Pavan Samudrala
metallization on PDMS
Barbara Cortese
2009-06-04
Your gold is too thick, try to reduce it, say more than 50%.

> The thickness of chrome was around 10nm and gold was around 100nm.
>
> Regards,
> Nidhi
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Harrick Plasma, Inc.
The Branford Group