MEMSnet Home: MEMS-Talk: About PMMA.....
About PMMA.....
1998-10-20
¹Úâ¹Î
About PMMA.....
¹Úâ¹Î
1998-10-20
Hello.
My question which chemical etches the PMMA.
I use PMMA as resist, And I want to remove PMMA some.
So to say, I have 100 nm thickness PMMA layer, and I want to
etch the PMMA about 30 nm thickness.
I know that the Oxygen RIE can this, but I want to know
the wet etching method not dry etching method.
I think some chemicals could do it.
I want to know which chemicals does that.
sincerely yours.
I wait your answer, thank you..
==================================================

==================================================
Æò»ý ¾²´Â ¹«·á E-mail ÁÖ¼Ò ÇѸÞÀϳÝ
http://www.hanmail.net


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics