1998-10-20
Antonella Benvenuto
About SU-8
Antonella Benvenuto
1998-10-20
--------------76DAD20E5D4037CF156D12F6
Content-Type: text/plain; charset=us-ascii
Content-Transfer-Encoding: 7bit

Dear MEMS researchers,
I'm now using EPON SU-8, but I have a problem to make a good adhesion
between the Si wafer (1 micron SiO2 layer on) and the SU-8.
Please does anyone tell me processing guide lines about?
Thank you very much,
Antonella


-----------------------------------
Antonella Benvenuto
Electronic Eng.
Mitech Lab-Scuola Superiore Sant'Anna
Via Carducci 40
56127 Pisa- Italy
Tel +39 050 883403
Fax +39 050 883402
e-mail: [email protected]
-----------------------------------


--------------76DAD20E5D4037CF156D12F6
Content-Type: text/html; charset=us-ascii
Content-Transfer-Encoding: 7bit


Dear MEMS researchers,

I'm now using EPON SU-8, but I have a problem to make a good adhesion between the Si wafer (1 micron SiO2 layer on) and the SU-8.
Please does anyone tell me processing guide lines about?
Thank you very much,
Antonella
 

-----------------------------------
Antonella Benvenuto
Electronic Eng.
Mitech Lab-Scuola Superiore Sant'Anna
Via Carducci 40
56127 Pisa- Italy
Tel +39 050 883403
Fax +39 050 883402
e-mail: [email protected]
-----------------------------------
  --------------76DAD20E5D4037CF156D12F6--

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Process Variations in Microsystems Manufacturing
Addison Engineering