MEMSnet Home: MEMS-Talk: How to peel off PDMS
How to peel off PDMS
2009-07-23
Shah, Forum N
2009-07-27
Sebastian Sosin - EWI
How to peel off PDMS
Shah, Forum N
2009-07-23
Hello All,

I am using Jersey cote for peeling off PDMS (about 50 micron) from Silicon
wafer.

It is peeling off but I am not able to peel it off as a continuous intact layer.
I am using a tweezer to peel it off.

If someone can suggest a way to peel it off intact it would be great.

Thanks in advance,
Forum