A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Source for Low Stress Silicon Nitride
Source for Low Stress Silicon Nitride
2009-08-17
Roger Shile
2009-08-17
antwi nimo
2009-08-18
Prasanna Srinivasan
2009-08-18
walter
2009-08-18
antwi nimo
2009-08-25
xudehui0108
Source for Low Stress Silicon Nitride
antwi nimo
2009-08-18
PVD or CVD are similar.  even CVD is better because of the low stress he is
after.


--- On Tue, 8/18/09, walter  wrote:

From: walter 
Subject: Re: [mems-talk] Source for Low Stress Silicon Nitride
To: [email protected], "General MEMS discussion" 
Date: Tuesday, August 18, 2009, 7:44 AM

Hi I don't know whether LPCVD will do the trick,also depending how thick a film.
You may want to consider PVD sputtering.

It worked well for us.

[email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.