MEMSnet Home: MEMS-Talk: Error in Oxygen Plasma Etching
Error in Oxygen Plasma Etching
2009-09-14
sniper
Error in Oxygen Plasma Etching
sniper
2009-09-14
Hi,

 Recently someone mistakenly etched my wafer coated with aluminum through oxygen
plasma etching.

 I probed the wires and found none of them are electrical conductive anymore.

 Maybe the top layer of the aluminum has been oxidized.

 Is there any way to safely eliminate this layer of alumina without harm the
under layers that contain gold silver and SiO2?

 Will the phosphoric acid (H3PO4) do the job?

 Thanks!

 Hao
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation