MEMSnet Home: MEMS-Talk: Re: Teflon adhesion
Re: Teflon adhesion
1998-10-21
[email protected]
1998-10-23
[email protected]
Re: Teflon adhesion
[email protected]
1998-10-23
Might try an Ar plasma pretreatment.

Gordon Whitlock
[email protected]


reply