MEMSnet Home: MEMS-Talk: Lithium evaporation?
Lithium evaporation?
2009-09-28
James Paul Grant
2009-10-09
Rais Nurgalejevs
Lithium evaporation?
Rais Nurgalejevs
2009-10-09
Hi James,

We use Lithium evaporation and diffusion, but without Au films.

What purpose?

Best regards,

Rais Nurgalejevs,
Engineer,
Riga
LATVIA