MEMSnet Home: MEMS-Talk: Re: Emissivity Tables for Silicon
Re: Emissivity Tables for Silicon
1998-10-21
[email protected]
1998-10-21
Ram N. Ramanan
1998-10-21
Fahrettin Levent Degertekin
Re: Emissivity Tables for Silicon
Fahrettin Levent Degertekin
1998-10-21
Since emissivity is important for optical temperature measurement
techniques, several researchers have measured this parameter. You can look
at a paper by P.J. Timans in Journal of Applied Physics, vol.74, no.10,
pp.6353-64, Nov. 1993 as a starting point.

Levent

 On Mon, 5 Oct 1998, Baird,
Deanna wrote:

> Has anyone written emissivity tables for silicon within your organization?
> Since the emissivity changes with heat, I would expect this may be difficult
> to measure.
>
> Any help you can provide would be helpful.
>
> Thank you.
>
> Regards,
> Deanna
>
> Deanna Baird
> FLIR Systems, Inc
> Manager - Applications
> 16505 SW 72nd Avenue
> Portland, OR 97224
> (503)684-3731 ext 833
>
>
>
***********************************
F. Levent Degertekin
E.L. Ginzton Laboratory
Stanford University
Stanford, CA 94305
Ph: (650) 723-8447
Fax: (650) 725-7509
email: [email protected]
Web: http://acoustics.stanford.edu
***********************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Process Variations in Microsystems Manufacturing
University Wafer