Dicing Polyimide Layer
2009-11-03
jianqiang gu
2009-11-03
Dave Lewis
2009-11-03
DongJuan Xi
2009-11-03
jianqiang gu
Dicing Polyimide Layer
Dave Lewis
2009-11-03
With features that small, you may be better off laser cutting the parts.
Dicing through the silicon tends to affect the optical characteristics
of the part especially areas closer to the saw.

Regards,
Dave Lewis


-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of jianqiang gu
Sent: Tuesday, November 03, 2009 2:15 AM
To: [email protected]
Subject: [mems-talk] Dicing Polyimide Layer

Hi Everybody,

Does anyone have experience with dicing hard cured polyimide layer
(PI2525, HD Microsystems)? I have a silicon wafer covered by a 100um
thickness hard cured PI2525 layer. I have to cut the polyimide layer
into 5mm*5mm pieces by my dicing saw. I'm wondering which kind of blade
I should choose and what is the proper spindle speed of the saw?

Thanks in advance.
Jianqiang Gu
Oklahoma State Univ.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMS Technology Review