Laser cutting of silicon
Vijay Rajaraman - EWI
2009-11-03
Hi Natsuki,

One trick you can try is to perform edge grinding of your laser cut wafers.

Regards,
Vijay
(TU Delft, NL)

-----Original Message-----
From: [email protected] [mailto:[email protected]] On
Behalf Of Miyakawa, Natsuki
Sent: dinsdag 3 november 2009 15:32
To: General MEMS discussion
Subject: [mems-talk] Laser cutting of silicon

Dear all,

After cutting silicon wafer with laser (frequency-tripled Nd:YAG-laser with wave
length 355nm) I observe that the silicon surface turned quite rough around the
cutting edge (height up to ~1µm, width ~ 50µm). Do you know some trick to avoid
or remove this surface roughening so that the surface quality is good enough for
silicon fusion bonding after laser cutting?

Thank you!

Cheers

Natsuki
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Addison Engineering
Process Variations in Microsystems Manufacturing