MEMSnet Home: MEMS-Talk: Replacement of critical point drying
Replacement of critical point drying
2009-11-06
lin yu
2009-11-07
Jie Zou
2009-11-08
Edward Sebesta
2009-11-08
Shay Kaplan
Replacement of critical point drying
Jie Zou
2009-11-07
What is your sacrificial layer? What liquid did your sample sit in before CPD?

In my case, I need to etch the oxide with 49% HF. So the sample is in
DI water after the HF releasing. The company MEMSCAP suggests to
replace the DI water with Isopropanol and then put it into oven to get
rid of Isopropanol. Isopropanol is supposed to generate much less
surface force than DI water.

Anyway, I never used that process since we have a quite good critical
point dryer. I think if you believe your beam is strong, maybe you
should try the process I just mentioned.


Jie


On Fri, Nov 6, 2009 at 2:01 PM, lin yu  wrote:
> Hi all,
>
> I'm trying to suspend a beam structure with 150nm wide and 10um long
> with critical point drying process. However, our CPD equipment is very
> violent while introducing liquid CO2. After this process, all the suspended
> beams are gone. So I was wondering if there's a possible replacement of
> CPD process to suspend beam structures. I heard that people use some
> kind of low surface tension liquid and air dry the samples. Does anyone have
> experience on this? Any suggestion is appreciated.
>
> Thanks,
> Lin

*  Zou Jie (Jay)
*  Department of Physics
*  University of Florida
*  Tel: +1-352-846-8018
*  Email: [email protected]
*  Homepage: http://plaza.ufl.edu/zoujie/
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Addison Engineering
University Wafer
Tanner EDA by Mentor Graphics