I am trying to do electroless Cobalt plating. I tried to find vendors
who sell the solution but except for Caswell Plating, no one else sells
it. I tried the one bought from Caswell but it does not work very well.
I am curious if anyone has some more information on it or some
experience with Cobalt plating. Thanks!!

-Rahul
([email protected])
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing
The Branford Group