MEMSnet Home: MEMS-Talk: PDMS surface treatment
PDMS surface treatment
2010-02-09
DEBASHIS MAJI
2010-02-09
Shirla Cheng
2010-02-11
DEBASHIS MAJI
PDMS surface treatment
Shirla Cheng
2010-02-09
DEBASHIS MAJI,

I have used both piranha and plasma to treat PDMS surfaces. If you want to use
piranha, the treatment time should be controlled to 10-15 sec. And the treatment
time with plasma (dry air or O2) should be 40-50 sec, otherwise the surface of
PDMS will be hardened and crack.

After piranha or plasma treatment, the PDMS surface is highly hydrophilic and
after that it will gradually become hydrophobic again.

Just for your reference.

Shirla Cheng


======= 2010-02-09 06:38:07 You wrote:=======

>Hi all,
>
>I would like to know whether anybody has any information regarding surface
>treatment of PDMS with piranha solution. Also is it as effective as plasma
>treatment? I shall be highly obliged if anyone can help me out in this and
>provide some material.
>
>Thanks in advance.
>
>Debashis Maji,
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.