Bromobenzene can be used for top-surface treatment of PR for lift-off process,
too. However, I don't know if it is any safer than chlorobenzene. I hope
someone can comment on the toxicity of bromobenzene......

Prof. CJ Kim
Micro-Manufacturing Laboratory
Mechanical, Aerospce, and Nuclear Engineering Department
University of California, Los Angeles


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing
University Wafer