MEMSnet Home: MEMS-Talk: Cleaning after wafer dicing
Cleaning after wafer dicing
2010-05-07
Miyakawa, Natsuki
2010-05-07
Jie Zou
2010-05-10
Thorsten Knoll
Cleaning after wafer dicing
Miyakawa, Natsuki
2010-05-07
Dear all,

After dicing my bonded wafers (glass with Si) I found out that my
microchannels covered by glass wafer got partially stuffed up by dicing
dust. The problem is that I have openings on the cut face so there is no
possiblity to protect them from cooling wafer with dice dust.

My question is, is there any method to removed the trapped dicing dust
from microchannels covered by bonded chip? I tried ultrasonic-bath with
alcohol, but it dind't help much.

Thank you!

Regards

Natsuki

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
The Branford Group
Process Variations in Microsystems Manufacturing