MEMSnet Home: MEMS-Talk: Re: Looking for AllResist company
Re: Looking for AllResist company
1998-10-30
Kai Hiltmann
1998-10-29
Jayant Neogi
Re: Looking for AllResist company
Jayant Neogi
1998-10-29
Claude:

MicroChem does supply three different AMU's (200k, 495k and 950k) of PMMA.
Our company has been ordering PMMA from this company. Also just wanted to
let you know briefly about our company, that we have developed the Maskless
Ion beam implantation technique using FIB's and have the capabilities to
generate sub-20 nm diffraction grating. We do provide a full line of
services in MEMS, Micromachining, Wet/dry chemical etching, electroplating,
and spincoating. We also sell 3 grades of PMMA developer that is very
sensitive to ion and ebeam exposure and shows excellent resolution. Let us
know if we could be of any assistance in future.

Regards
Jayant
**********************************************************
Jayant Neogi
Director: Research and Development
NORSAM Technologies
Ph#  (503) 640-0586
Fax# (503) 640-8117
************************************************************
-----Original Message-----
From: Claude Beaulieu 
To: [email protected] 
Date: Thursday, October 29, 1998 9:40 AM
Subject: Looking for AllResist company


>
>
>I'm trying to contact a company that sell a PMMA solution as electron
>beam resist. The company name is AllResist and is located in Berlin,
Germany.
>
>Does anybody know the phone#, fax#, or e-mail contact for this company.
>
>Also if you know other suppliers of PMMA resist, I'm interrested too.
>
>My work involved submicron diffractive optical elements in fused silica.
>
>
>
>
>Claude Beaulieu
>
>QPS Technology Inc.
>2270 St-Francois
>Dorval, Quebec
>H9P 1K2
>Canada
>
>Tel.:514 421 7558 (ext.:32)
>Fax :514 421 7370
>
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
The Branford Group
MEMStaff Inc.