A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Porous Silicon recipe
Porous Silicon recipe
2010-09-17
ANIRBAN SARKAR
2010-09-19
antwi nimo
Porous Silicon recipe
ANIRBAN SARKAR
2010-09-17
Hello all,

 I have been trying to generate porous silicon for our project but I am not
being able to obtain porous Silicon in the range of 50nm to 200nm.
I am requesting some insight in the recipe of generation of porous Si.

Any help will be gladly appreciated.

Thanks
Anirban

Electrical Engineering
Louisiana State University
Baton Rouge
70802,USA
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
The Branford Group
Process Variations in Microsystems Manufacturing