MEMSnet Home: MEMS-Talk: AMMT KOH etch wafer holder
AMMT KOH etch wafer holder
2010-09-30
Bhargav Nabar
2010-10-01
Kuijpers, Peter
2010-10-01
Bhargav Nabar
2010-10-04
Kuijpers, Peter
AMMT KOH etch wafer holder
Bhargav Nabar
2010-10-01
Thank you for your suggestion Mr Kuijpers. Could you please comment on ease
of removal of the parylene layer. What solvent do you use and does
it require any agitation (slow rotating or ultrasonic?). Also how was you
experience with the silicet clamp?

Thank you once again.
Bhargav Nabar
UT Arlington Nanofab
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
University Wafer