Dear all:

   Our dektak stylus profiler has encountered a malfunction when lowering
the tower (needle). It keeps noticing that "the tower does not lower
down...". Restart the facility can't solve this problem. (the facility is
kind of old)

   Our technician is on sick leave. and we can't fix it.
   Does anyone how to fix such kind of problem? Many thanks!

--
Sincerely
Jack, Zetao MA
Dept.of EEE, CYC712,HKU
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics