MEMSnet Home: MEMS-Talk: Uneven surface thickness of SU-8 2100
Uneven surface thickness of SU-8 2100
2010-12-01
Nirmal punjabi
2010-12-01
Alex Mellnik
2010-12-02
[email protected]
2010-12-02
Xiaohui Lin
2010-12-02
Michael Riss
Uneven surface thickness of SU-8 2100
Xiaohui Lin
2010-12-02
Just spin on the whole wafer then cut out the central even area for use.

Or you need special spin tools with bead removal.

On Wed, Dec 1, 2010 at 11:30 AM, Nirmal punjabi wrote:

> Hi,
>
> I need a thickness of around 400um of SU-8, i am spin coating SU-8 2100 at
> 800rpm for 60 sec.
>
> But the final structure formed has uneven surface.
>
> Can anyone help me on this matter?
>
> Thank you.
>
> Nirmal.

--
Lin, Xiaohui
Ph.D. Program in Electrical and Computer Engineering
Nanophotonics and Optical Interconnects Group
Microelectronics Research Center
The University of Texas at Austin
E-mail: [email protected]
Office: (512) 471-4349
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing
The Branford Group