A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Protek adhesion problem
Protek adhesion problem
2011-02-07
Temmuz
2011-02-07
Warren Dustin
2011-02-08
Bill Moffat
Protek adhesion problem
Warren Dustin
2011-02-07
Hello Temmuz.

Usually an organosilane of some sort will help with the adhesion.  You
can try a dehydration bake followed by application of HMDS.  When I used
Protek I used an adhesion promoter with good results from HD
Microsystems.

Good luck.

Best Regards,

Dustin Warren, PE

EV Group
invent * innovate * implement
Strategic Account Manager North America - Direct: +1 (480) 305 2447,
Main: +1 (480) 305 2400 Fax: +1 (480) 305 2401
Cell: +1 (480) 274 3894
E-Mail: [email protected], Web: www.EVGroup.com


-----Original Message-----
From: Temmuz [mailto:[email protected]]
Sent: Monday, February 07, 2011 5:39 AM
To: [email protected]
Subject: [mems-talk] Protek adhesion problem

Hi,

I am trying to etch 500um Si wafer with %30 KOH at 80C.  I bought Protek

PSB coating in order to protect my front side however the adhesion is
very bad.  Does anybody have intel about this issue and how to overcome?

Thanks in advance

Temmuz CEYHAN
M.Sc. Student
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search