MEMSnet Home: MEMS-Talk: chemical formula of Futurrex NR9 photoresist
chemical formula of Futurrex NR9 photoresist
2011-02-15
Hong Wang
chemical formula of Futurrex NR9 photoresist
Hong Wang
2011-02-15
Anyone has idea what is the chemical formula NR9 photoresist?

Futurrex NR9-8000 is a negative, polyhydroxy-styrene based photoresist
designed for i-line applications.

Thanks,

Hong