Xiaohui Lin
2011-04-27
[email protected]
Ni electroplating of < 1 um
[email protected]
2011-04-27
Hi,
I was electrodepositing Ni at a nanometer scale. It depends on
solution used, Voltage applied,  substrate etc.

But if you find the right parameters you fey very uniform thin layers

La data de 26.04.2011, 22:55, Xiaohui Lin  a
scris:

> Does anyone have experience electroplating Ni with thickness less than
> 1um? How is the uniformity and surface roughness?

> Thanks.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Mentor Graphics Corporation