MEMSnet Home: MEMS-Talk: wet etching of fused silica
wet etching of fused silica
2011-06-27
Kuijpers, Peter
2011-06-27
Mac McReynolds
wet etching of fused silica
Kuijpers, Peter
2011-06-27
Hi all,

I want to wet etch a some trenches into fused silica wafers.
Depth is app. 200µm and also  width is app 200µm.
What material can I use for masking  can I use and which etchant?

Many thanks in advance.


Peter Kuijpers
Process Engineer
Philips Innovation Services
MiPlaza/TL group
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation