Thomas Reddy
2011-07-21
Shay
2011-07-21
Khawar Abbas
Quartz wafer dicing
Shay
2011-07-21
Anyone with a dicing saw can do this for you. You might want to coat the
Cr-Au with resist to avoid micro scratches.

Shay

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Thomas
Reddy
Sent: Thursday, July 21, 2011 6:47 AM
To: [email protected]
Subject: [mems-talk] Quartz wafer dicing

Hi everyone,

Does anyone know how I can dice my 4" quartz wafer to quarter pieces?
I should mention that I have a Cr-Au layers on my wafer and don't know that
is it possible to find any way for protecting them? Does fluid and soup of
the dicing saw damage my Cr-Au layers?

Regards,
Thomas
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
Nano-Master, Inc.
Tanner EDA by Mentor Graphics