MEMSnet Home: MEMS-Talk: dicing particle contamination
dicing particle contamination
2012-07-24
ProtoSi Info
2012-07-25
Gabriel Puebla-Hellmann
2012-07-25
[email protected]
2012-07-25
Carel Heerkens - TNW
2012-07-25
Yingtao Tian
2012-07-25
Bill Moffat
2012-07-26
Mark West
dicing particle contamination
Gabriel Puebla-Hellmann
2012-07-25
Hi,

We've also seen issues with this when dicing sapphire wafers. I usually
strip the resist with the chip upside-down, which works most of the time. An
alternative used in our lab is a two layer resist, first PMMA 950K, then
standard positive photoresist. After dicing, the photo resist is stripped
with developer, ideally stirring the chips upside down, which removes most
particles. The pmma layer is then removed using acetone, which also removes
the remaining particles. Beware of pmma residue though.

Hope this helps,

Gabriel

Quantum Device Lab, ETHZ



-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of
ProtoSi Info
Sent: Tuesday, July 24, 2012 9:22 PM
To: [email protected]
Subject: [mems-talk] dicing particle contamination

Hello

We've been struggling with particles getting embedded in our delicate
silicon comb structures during dicing. Our current process involves spraying
on a 10um thick layer of photoresist over the entire wafer and then do a
soft bake. After dicing we rinse the wafer to remove particles before
stripping off the resist. However we're still getting particles stuck
in-between the comb fingers. We've attempted ultrasonic cleaning but that
damages the combs.

Any tips to remove or prevent particles would be greatly appreciated.

Thank you
Kevin Chang
ProtoSi
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk


_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing