A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Spin-coating of thick photoresist over existing features
Spin-coating of thick photoresist over existing features
2012-12-20
João Tiago dos Santos Fernandes
2012-12-20
Gary Hillman
2012-12-20
Felix Lu
2012-12-21
Gareth Jenkins
2012-12-21
Lukasz Urbanski
2012-12-26
João Tiago dos Santos Fernandes
2012-12-26
Black, Robert
Spin-coating of thick photoresist over existing features
Lukasz Urbanski
2012-12-21
this may help:

http://microchem.com/su_eight_faq.htm

Happy Holidays


2012/12/20 Gareth Jenkins :
> Perhaps try covering the wafer in the resist solvent before pouring the
> resist? This may help fill the gaps.
>
> On 21 December 2012 02:57, João Tiago dos Santos Fernandes <
> [email protected]> wrote:
>
>> Hi everyone,
>>
>> I'm currently using AZ 40XT thick photoresist to make a 20-30 µm thin film
>> over a Si sample with ~30 µm high SU-8 features.
>>
>> The problem I am facing is the following: when I pour the AZ on top of the
>> sample, tiny air-bubbles are created in areas where SU-8 features are small
>> (small wells, gaps, etc) - I'm guessing that this happens because the AZ is
>> very viscous and isn't able to fill those spaces and traps air. When I spin
>> coat, those tiny air bubbles are spread across the sample, compromising the
>> process.
>>
>> Is there any way to get the air bubbles out of the way without
>> compromising the final film thickness? I tried low rpm for a couple of
>> minutes, with no success.
>>
>> Thank you so much,
>>
>> -----------------------------
>> João Tiago dos Santos Fernandes
>>
>> INESC Microsistemas e Nanotecnologias (INESC MN)
>> Rua Alves Redol, 9
>> 1000-029 Lisboa
>> Portugal
>>
>> Tel: +351 213100237
>> Email: [email protected]
>> URL: www.inesc-mn.pt
>>
>> _______________________________________________
>> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
>> provider of MEMS and Nanotechnology design and fabrication services.
>> Visit us at http://www.mems-exchange.org
>>
>> Want to advertise to this community?  See http://www.memsnet.org
>>
>> To unsubscribe:
>> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>>
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
The Branford Group
Process Variations in Microsystems Manufacturing