Hello all,

I am new in this forum and I found really interesting.
I want to etch the bottom of SOI wafer 550um in LF. I have the same
problem with grass or black silicon.
I used some Si bulk wafer to do it first and it is really hard to do it
without hard mask. Has anyone any idea about
it ? I am using SPR photoresist
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing