MEMSnet Home: MEMS-Talk: supplier for low-price hot press/embosser
supplier for low-price hot press/embosser
2013-07-18
Shane
2013-07-18
Tong CHEN
2013-07-22
Gareth Jenkins
supplier for low-price hot press/embosser
Gareth Jenkins
2013-07-22
Have a look at Carver Press (www.carverpress.com). There are a few groups
using these for microfluidic embossing with good results.

On 18 July 2013 11:12, Shane  wrote:

> Hello everyone,
>
> Can you share some information about suppliers that sell low-price hot
> press for polymer replica molding? Hot embosser is also fine but I believe
> a programmable hot embosser with automatic control and a dedicated cooling
> unit can be quite expensive. We are looking for some cheap alternatives
> that can be used for molding thermalplastic microfluidic devices.
>
> cheers
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing