MEMSnet Home: MEMS-Talk: adhesion agents
adhesion agents
2013-09-18
Fahd Ali
2013-09-18
Bill Moffat
2013-09-18
Gary Hillman / S-Cubed
2013-09-19
Kevin Nichols
2013-09-20
Fahd Ali
2013-09-20
Bill Moffat
2013-09-18
Gary Hillman / S-Cubed
adhesion agents
Fahd Ali
2013-09-18
Hi,
I am searching for a silane coupling agent for the bonding of glass and polymer
(FEP films) . For bonding purposes I have to go up to 260°C, are there coupling
agents or adhesives available which can stand this temperature.

kind regards,
-----------------------------------------------
Fahd Ali


_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Harrick Plasma, Inc.
Addison Engineering