MEMSnet Home: MEMS-Talk: Prevention of anodic bonding using Chrome
Prevention of anodic bonding using Chrome
2013-12-20
Deep Mukhopadhyay
Prevention of anodic bonding using Chrome
Deep Mukhopadhyay
2013-12-20
Dear Members:

I have heard that one can prevent anodic bonding between Glass and Silicon
Dioxide using Chrome.

Does the Chrome need to be deposited on Glass, or can I deposit Chrome on
Silicon Dioxide, to prevent anodic bonding from taking place?

Regards,

-Deep

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
MEMS Technology Review
Harrick Plasma, Inc.